Polymer Property : Flexural Modulus = 30.2 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 30.2 GPa
4380 ksi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Flexural Modulus 30.2 GPa
4380 ksi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..