Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.447 GPa | 499.9 ksi | XY; ASTM D790 |
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized.. |