Polymer Property : Flexural Modulus = 3.186 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.10 - 3.186 GPa
450 - 462.1 ksi
90 Minute UV Cure + Thermal; ASTM D790
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..
Flexural Modulus 2.827 - 3.186 GPa
410.0 - 462.1 ksi
ASTM D790
3D Systems Accura® 10 Plastic for SLA® Systems
Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsGeneral use prototyping for many uses, including:Enclosures, covers and casesCellular/mobile ph..