Material Notes:
Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsGeneral use prototyping for many uses, including:Enclosures, covers and casesCellular/mobile phonesAutomotive and aerospace designComputers and control displaysAccurate master patterns for RTV/silicone moldingQuickCast™ patterns for investment castingModels for fluid flow and visualization of internal structuresAll information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.16 g/cc

@Temperature 25.0 °C
0.0419 lb/in³

@Temperature 77.0 °F
Liquid
1.21 g/cc

@Temperature 25.0 °C
0.0437 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 485 cP

@Temperature 30.0 °C
485 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength, Yield 62.0 - 76.0 MPa
8990 - 11000 psi
ASTM D638
Elongation at Break 3.1 - 5.6 %
3.1 - 5.6 %
ASTM D638
Tensile Modulus 3.048 - 3.532 GPa
442.1 - 512.3 ksi
ASTM D638
Flexural Strength 89.0 - 115 MPa
12900 - 16700 psi
ASTM D790
Flexural Modulus 2.827 - 3.186 GPa
410.0 - 462.1 ksi
ASTM D790
Izod Impact, Notched 0.149 - 0.277 J/cm
0.279 - 0.519 ft-lb/in
ASTM D256
Penetration 6.3
6.3
mils; Viper/SLA 3500
6.8
6.8
mils; SLA 7000
6.9
6.9
mils; SLA 5000
Thermal Properties Metric English Comments
CTE, linear 64.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
35.6 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
170 µm/m-°C

@Temperature 90.0 - 150 °C
94.4 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C
136 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Glass Transition Temp, Tg 62.0 °C
144 °F
DMA, E"
Descriptive Properties Value Comments
Appearance Clear amber
Critical Exposure (mJ/cm²) 13.8
Viper/SLA 3500
15.5
SLA 7000
17.7
SLA 5000
Tested Build Styles FAST™, EXACT HR, QuickCast™ and ThinLayer™