Polymer Property : Flexural Modulus = 29.460 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.20312 - 0.20312 GPa

@Temperature 204 - 204 °C
29.460 - 29.460 ksi

@Temperature 400 - 400 °F
Average value: 0.203 GPa Grade Count:1
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..