Mechanical Properties Metric English Comments
Flexural Modulus 0.201 GPa
29.2 ksi
ASTM D790
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase