Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.201 GPa | 29.2 ksi | ASTM D790 |
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |