Mechanical Properties Metric English Comments
Flexural Modulus 19.6 GPa
2840 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific)
CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 19.6 GPa
2840 ksi
ASTM D790
Kostat E-3007J Conductive PS Compound
KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea..
Flexural Modulus 19.6 GPa
2840 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA..
Flexural Modulus 19.6 GPa
2840 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Europe-Africa-Middle East)
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 19.6 GPa
2840 ksi
GB/T 9341-2008
Sichuan Deyang Haton® hGR60 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Modulus 19.6 GPa
2840 ksi
ASMT D790
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced
Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel..
Flexural Modulus 19.6 GPa
2840 ksi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Fibre Glast ProSet 125R / 229H Epoxy  (discontinued **)
Information provided by Fibre Glast Developments Corporation.