Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.961 GPa | 284.4 ksi | ASTM D790 |
Kolon KOPA® KN333NW High Impact Nylon 66 Impact -resistant, dimensional safetyApplications Wheel coversInformation provided by API-Kolon. |
|||
Flexural Modulus | 1.961 GPa | 284.4 ksi | ASTM D790 |
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin High elastic, whether resistantApplications: WipersInformation provided by API-Kolon. |