Flexural Modulus 19.13 GPa
2775 ksi
ASTM D790
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced
Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..