Mechanical Properties Metric English Comments
Flexural Modulus 25.9 GPa
3760 ksi
ASTM D790
PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 25.9 GPa
3760 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Flexural Modulus 25.9 GPa
3760 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..