Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.3 GPa | 2360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP LCL36 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL36 is a compound based on Polyetheretherketone containing Carbon Fiber , PTFE. Added features of this material include Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 16.3 GPa | 2360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 16.3 GPa | 2360 ksi | ASTM D790 |
Plenco 6990 Phenolic, Briquette, Transfer Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Flexural Modulus | 16.3 GPa | 2360 ksi | ASTM D790 |
Unitika RUN35-C25 Weather resistant PA6, Dry Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd. |