Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Unitika
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika RUN35-C25 Weather resistant PA6, Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 1.05 %
1.05 %
50% RH
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength at Break 171 MPa
24800 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Tensile Modulus 18.4 GPa
2670 ksi
ASTM D638
Flexural Strength 247 MPa
35800 psi
ASTM D790
Flexural Modulus 16.3 GPa
2360 ksi
ASTM D790
Izod Impact, Notched 0.470 J/cm
0.881 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 1.50 µm/m-°C
0.833 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
383 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
415 °F