Mechanical Properties Metric English Comments
Flexural Modulus 16.13 GPa
2339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp GC006XXZ PSU
LNP THERMOCOMP* GC006XXZ is a compound based on Polysulfone resin containing Carbon Fiber.This product is also known as Thermocomp* GC-1006.This data was supplied by SABIC-IP for the Americas region..