Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.13 GPa | 2339 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp GC006XXZ PSU LNP THERMOCOMP* GC006XXZ is a compound based on Polysulfone resin containing Carbon Fiber.This product is also known as Thermocomp* GC-1006.This data was supplied by SABIC-IP for the Americas region.. |