Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.159 GPa | 23.0 ksi | ASTM D790 |
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |