Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.85 GPa | 2299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Flexural Modulus | 15.85 GPa | 2299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Flexural Modulus | 15.85 GPa | 2299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 15.85 GPa | 2299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI (Asia Pacific) LNP* Thermocomp* ECF62 is a compound based on Polyetherimide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 15.85 GPa | 2299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |