Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.96 GPa | 2170 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear .. |
|||
Flexural Modulus | 14.96 GPa | 2170 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 15.0 GPa | 2170 ksi | ASTM D570 |
Solvay Specialty Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled
(discontinued **)< XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and .. |