Mechanical Properties Metric English Comments
Flexural Modulus 1.502 GPa
217.8 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers SBS 1001 Styrene Butadiene Block Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.