Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 21.6 GPa | 3130 ksi | ASTM D790 |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |