Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 21.448 GPa | 3110.8 ksi | ASTM D-790 |
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |