Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.39 GPa | 202 ksi | 1% Secant; ASTM D790 |
Flint Hills P9H9Z-018 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ISO 178 |
Lucite International Diakon® TD642 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ASTM Test |
Styrolution Styrolux HS 70 SBC Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific) LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | ISO 178 |
Cathay PA513 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Flexural Modulus | 1.39 GPa | 202 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® 4082 Polypropylene, Injection Grade Bapolene PP4082 is a high flow, fast cycle injection molding resin. Injection molded parts exhibit good stiffness and chemical resistance. This product meets FDA standards for food contact applica.. |