Bapolene® 4082 Polypropylene, Injection Grade

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 4082 Polypropylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP4082 is a high flow, fast cycle injection molding resin. Injection molded parts exhibit good stiffness and chemical resistance. This product meets FDA standards for food contact applications.Applications: Thin-walled articles, caps, closures, and medical devices.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ASTM D-2240
Tensile Strength, Ultimate 19.3 MPa
2800 psi
2 in/min (50 mm/min); ASTM D638
Tensile Strength, Yield 35.9 MPa
5210 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 490 %
490 %
2 in/min (50 mm/min); ASTM D638
Elongation at Yield 21 %
21 %
2 in/min (20 mm/min); ASTM D638
Flexural Modulus 1.39 GPa
202 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved