Polymer Property : Flexural Modulus = 2.497 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.497 GPa
362.2 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers ASAPC 130 UV Stabilized
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.497 GPa
362.2 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers ASAPC GLY 130 UV Stabilized
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.