Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASAPC 130 UV Stabilized

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASAPC 130 UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.497 GPa
362.2 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 137 °C

@Load 1.00 kg,
Thickness 3.17 mm
279 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Users viewing this material also viewed the following: