Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.412 GPa @Thickness 6.35 mm |
349.8 ksi @Thickness 0.250 in |
tangent; chs 2.5 in/min; 100 mm SL; ASTM D790 |
Diamond Polymers ABSPC 7030-HES ABS/PC Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |