Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.382 GPa | 345.5 ksi | ISO 178 |
S&E Specialty Polymers TufFillâ„¢ 5701 Black PP Application: High Calcium carbonate filed, high heat resistance thermoplastic extrusion grade based on polypropylene copolymer/homopolymer.Information provided by S&E Specialty Polymers |
|||
Flexural Modulus | 2.382 GPa | 345.5 ksi | ASTM D790 |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |