Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.70 - 2.20 GPa | 247 - 319 ksi | |
Prodways PLASTCure Clear 100 3D Printing Polymer Ultra clear.Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Wide range of medical applicationInformation provided by G.. |
|||
Flexural Modulus | 1.70 - 2.20 GPa | 247 - 319 ksi | |
Prodways PLASTCure Model 100 3D Printing Polymer Allows production of precise components; high workability.Used for dental applications from models for restorations to orthodontics.Information provided by Genistar. |
|||
Flexural Modulus | 1.70 - 2.20 GPa | 247 - 319 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Flexural Modulus | 2.00 - 2.20 GPa | 290 - 319 ksi | ASTM D790 |
Loxim 820 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 1.70 - 2.20 GPa @Temperature 60.0 - 120 °C |
247 - 319 ksi @Temperature 140 - 248 °F |
Average value: 1.88 GPa Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |