Polymer Property : Flexural Modulus = 2.103 GPa
Polymer Property :
Flexural Modulus =
2.103 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
2.103
GPa
305.0
ksi
ASTM D790
NYCOA 1417HS PA 6
impact modified, heat stabilized, medium high impact strengthInformation provided by NYCOA, Inc.