Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.059 GPa | 298.6 ksi | ASTM D790 |
Kolon KOPA® KN333HFBL General Purpose Nylon 66 Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon. |
|||
Flexural Modulus | 2.059 GPa | 298.6 ksi | ASTM D790 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Flexural Modulus | 2.059 GPa | 298.6 ksi | |
Kuraray HYBRAR® PS2 Thermoplastic Rubber-Polystyrene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |