Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kuraray HYBRAR® PS2 Thermoplastic Rubber-Polystyrene Blend

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber , Polystyrene (PS)
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® PS2 Thermoplastic Rubber-Polystyrene Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® and other polymers exhibit excellent vibration damping properties.Mixing Conditions: Twin screw extruder @ 200°CMolding Conditions: Injection Molding, Cylinder @ 200°C, mold @ 60°CFormulation (parts by weight): Polystyrene - 85, HYBRAR® 5127 - 15Information provided by The Kuraray Group.
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Tensile Strength, Ultimate 47.0 MPa
6820 psi
Elongation at Break 21 %
21 %
Tensile Modulus 2.157 GPa
312.9 ksi
Flexural Strength 28.0 MPa
4060 psi
Flexural Modulus 2.059 GPa
298.6 ksi
Descriptive Properties Value Comments
Loss Factor 0.04
measured by resonance method with a cantilever beam
Tan Delta 0.047
at 0°C, measured w/ Rheovibron @ 11 Hz
0.063
at 40°C, measured w/ Rheovibron @ 110 Hz
0.075
at 25°C, measured w/ Rheovibron @ 110 Hz