Polymer Property : Flexural Modulus = 198 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.37 GPa
198 ksi
12.5 mm/min; ASTM D790
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Flexural Modulus 1.37 GPa
198 ksi
ASTM D790
LyondellBasell Moplen HP400H Polypropylene Homopolymer
Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications ..
Flexural Modulus 1.36 - 3.38 GPa
198 - 490 ksi
Average value: 2.11 GPa Grade Count:71
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..