Polymer Property : Flexural Modulus = 1881 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.97 GPa
1881 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp UCL24S PPA (Asia Pacific)
LNP* Lubricomp* UCL24S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond..