SABIC Innovative Plastics LNP Lubricomp UCL24S PPA (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp UCL24S PPA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* UCL24S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Conductive.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 162 MPa
23500 psi
ASTM D 638
Elongation at Break 1.7 %
1.7 %
ASTM D 638
Flexural Strength 248 MPa
36000 psi
ASTM D 790
Flexural Modulus 12.97 GPa
1881 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 3.49 J/cm

@Temperature 23.0 °C
6.54 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 248 °C

@Thickness 3.20 mm
478 °F

@Thickness 0.126 in
unannealed; ASTM D 648