Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.759 GPa | 1850.5 ksi | ASTM D-790 |
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |