Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.755 GPa | 1850.0 ksi | Tangent; ASTM D790 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |