Mechanical Properties Metric English Comments
Flexural Modulus 12.755 GPa
1850.0 ksi
Tangent; ASTM D790
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent ..