Mechanical Properties Metric English Comments
Flexural Modulus 2.50 - 12.8 GPa
363 - 1850 ksi
Average value: 5.56 GPa Grade Count:213
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..