Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.273 GPa | 184.6 ksi | ASTM D-790 |
Bapolene® 5010H High Density Polyethylene This resin is a high molecular weight, high density copolymer polyethylene resin. Product exhibits superior impact strength and ESCR. Resin contains a process stabilizer and complies with FDA 21 C.. |