Mechanical Properties Metric English Comments
Flexural Modulus 1.273 GPa
184.6 ksi
ASTM D-790
Bapolene® 5010H High Density Polyethylene
This resin is a high molecular weight, high density copolymer polyethylene resin. Product exhibits superior impact strength and ESCR. Resin contains a process stabilizer and complies with FDA 21 C..