Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790 |
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM202 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® SM850 Polypropylene impact copolymer Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790 |
Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.125 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | 0.079 in/min; ISO 178 |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |
|||
Flexural Modulus | 1.27 - 15.0 GPa | 184 - 2180 ksi | Average value: 6.70 GPa Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |