Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Glass Filled
Manufacturer Covestro
Trade Name Baydur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contains continuous strand fiberglass mat.0.125 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.510 g/cc
0.0184 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Bayer Test
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.0 MPa
3050 psi
ASTM D638/D412
Elongation at Break 1.7 %
1.7 %
ASTM D638/D412
Flexural Yield Strength 39.0 MPa
5660 psi
ASTM D790
Flexural Modulus 1.27 GPa
184 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696