Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 124 GPa | 18000 ksi | 0°; RT |
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |