Polymer Property : Flexural Modulus = 18.92 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00CE is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific)
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON RV00CES PA 66
LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific)
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON RX06424 PA 66
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural