Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON* RV00CE is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0041 cm/cm

@Time 86400 sec
0.0041 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 261 MPa
37900 psi
ISO 527
Elongation at Break 1.6 %
1.6 %
ISO 527
Tensile Modulus 23.28 GPa
3376 ksi
1 mm/min; ISO 527
Flexural Strength 433 MPa
62800 psi
ISO 178
Flexural Modulus 18.92 GPa
2744 ksi
ISO 178
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
43.0 kJ/m²

@Temperature -40.0 °C
20.5 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.44 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af