Polymer Property : Flexural Modulus = 18.77 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 18.77 GPa
2722 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10
LNP THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.