Polymer Property : Flexural Modulus = 18.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.125 GPa
18.1 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.125 GPa
18.1 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.125 GPa
18.1 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.125 GPa
18.1 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.125 GPa
18.1 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.125 - 0.300 GPa
18.1 - 43.5 ksi
Average value: 0.208 GPa Grade Count:7
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Flexural Modulus 0.125 GPa
18.1 ksi
ASTM D790
Toyobo Pelprene™ S-1001 Polyester TPE
Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block..
Flexural Modulus 0.125 GPa
18.1 ksi
ISO 178
Borealis LE6023 Polyethylene Modified Jacketing Compound
LE6023 is a black flexible low density copolymer modified polyethylene compound. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in..
Flexural Modulus 0.125 GPa
18.1 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.