Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.34 GPa | 1790 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 LNP* STAT-KON* RE004 is a compound based on Nylon 66 resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |