Mechanical Properties Metric English Comments
Flexural Modulus 12.34 GPa
1790 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66
LNP* STAT-KON* RE004 is a compound based on Nylon 66 resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.