POLYMER SEARCH
Polymer Property : Flexural Modulus = 1749.4 ksi
Polymer Property :
Flexural Modulus =
1749.4 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
12.062
GPa
1749.4
ksi
ASTM D790
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66
G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon.